Thread
:
Fusing/slumping/casting with kiln sitter
View Single Post
#
7
December 10th 03, 02:19 AM
nJb
external usenet poster
Posts: n/a
On Tue, 09 Dec 2003 19:00:07 GMT,
wrote:
On Sat, 06 Dec 2003 21:14:41 +1100, Greg Kraushaar
wrote:
I HAVE used a kiln sitter successfully for both Slumping and fusing.
Why? I have one and can't afford better.
It is true that they only control the Max temp, but they are very
accurate. Usually within a degree or so. (
And hope that the cone doesn't stick and over fire the kiln.
Just completed a glass cast 11KG which took 13 1/2 days kiln time.
I use a Perfect Fire III and I love it
Cheers
Jo
13-1/2 days. That's getting serious. The 200" mirror for the scope on
Mt Polomar took 11 months to cool. Josh Simpson's 12" diameter
"worlds" take about 4 months.
What were the dimensions of your casting?
Jack
http://photos.yahoo.com/bc/xmissionbobo/
nJb
Ads